Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 150 MPa
21800 psi
Test speed 100%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2
Mitsubishi Hostaphan® RN, 190 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin..
Film Tensile Strength at Yield, MD 150 MPa
21800 psi
Test speed 100%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2
Mitsubishi Hostaphan® RN, 250 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin..
Film Tensile Strength at Yield, MD 150 MPa
21800 psi
Test speed 100%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2
Mitsubishi Hostaphan® RN, 350 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin..
Film Tensile Strength at Yield, MD 150 MPa
21800 psi
ASTM D882
CEN® Electronic Material CV Polyimide Film, 4 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..
Film Tensile Strength at Yield, MD 150 MPa
21800 psi
CEN® Electronic Material CN Polyimide Film, 1 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..