Material Notes:
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film can be laminated, metallized, punched, formed or adhesive coated. CEN®CN is used for applications that require an all-polyimide film with an excellent balance of properties over a wide range of temperatures.Applications: mechanical parts, electronic parts, electrical insulation, pressure sensitive tape, fiber optics cable, insulation blankets, insulation tubing, automotive diaphragms sensors and manifolds.All information provided by CEN Electronic Material Co., LTD.
Physical Properties Metric English Comments
Thickness 22.0 - 28.0 microns
0.866 - 1.10 mil
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 150 MPa
21800 psi
Film Tensile Strength at Yield, TD 145 MPa
21000 psi
Film Elongation at Yield, MD >= 45 %
>= 45 %
Film Elongation at Yield, TD >= 45 %
>= 45 %
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Strength >= 200 kV/mm
>= 5080 kV/in