Polymer Property : Film Tensile Strength at Yield, MD = 2200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 15.2 MPa
2200 psi
ASTM D882
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin
Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL..
Film Tensile Strength at Yield, MD 15.2 MPa
2200 psi
ASTM D882
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin
Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL..
Film Tensile Strength at Yield, MD 15.2 MPa
2200 psi
ASTM D882
ExxonMobil LLDPE LL 3402.48 Cast Linear Low Density Polyethylene Resin
Product Description: LL 3402.48 is a hexane medium density polyethylene cast film grade for applications requiring high stiffness. It can also be used in blown films. Films produced from this resin ..
Film Tensile Strength at Yield, MD 15.2 MPa
2200 psi
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good..
Film Tensile Strength at Yield, MD 15.2 MPa
2200 psi
Dow LDPE 768A Low Density Polyethylene, Film Grade
DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a..
Film Tensile Strength at Yield, MD 15.2 MPa
2200 psi
ASTM D882
Bapolene® 200F Polyethylene, Film Grade
Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for foo..