Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 200F Polyethylene, Film Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 200F Polyethylene, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for food contact applications.Applications: General purpose clarity applications.Film properties below are based on a thickness of 32 µm and blow-up ratio of 2:1.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 32.0 microns
1.26 mil
2:1 blow-up ratio
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 15.2 MPa
2200 psi
ASTM D882
Film Tensile Strength at Yield, TD 12.4 MPa
1800 psi
ASTM D882
Film Elongation at Break, MD 360 %
360 %
ASTM D-882
Film Elongation at Break, TD 580 %
580 %
ASTM D-882
Secant Modulus, MD 0.193 GPa
28.0 ksi
0.1 mm/mm-min Initial strain rate; ASTM D-882
Secant Modulus, TD 0.207 GPa
30.0 ksi
0.1 mm/mm-min Initial strain rate; ASTM D-882
Elmendorf Tear Strength, MD 17.7 g/micron
450 g/mil
ASTM D-1922
Elmendorf Tear Strength, TD 8.30 g/micron
211 g/mil
ASTM D-1922
Dart Drop 2.46 g/micron
62.5 g/mil
26 in. dart; ASTM D-1709, A
Film Tensile Strength at Break, MD 22.8 MPa
3310 psi
ASTM D-882
Film Tensile Strength at Break, TD 17.9 MPa
2600 psi
ASTM D-882
Optical Properties Metric English Comments
Gloss 67 %
67 %
ASTM D-2457
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: