Film Tensile Strength at Yield, MD 25.0 MPa
3630 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PE 1291
PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Film Tensile Strength at Yield, MD 25.0 MPa
3630 psi
ASTM D882
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin
Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Film Tensile Strength at Yield, MD 25.0 MPa
3630 psi
ASTM D882
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin
Features: Excellent barrier propertiesHigh stiffnessGood processability Low gel Applications: Barrier filmsCo-extrusionDry food packagingInformation provided by Nova Chemicals
Film Tensile Strength at Yield, MD 25.0 - 30.0 MPa
3630 - 4350 psi
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents..
Film Tensile Strength at Yield, MD 25.0 MPa
3630 psi
ASTM D882
Chevron Phillips K-Resin® KR53 Styrene-Butadiene Copolymer
Customer Benefits:Excellent ClarityHigh Surface GlossGood ToughnessGood Heat SealabilityTypical Applications:Medical PackagingProduce PackagingTwist WrapLidstock and Labeling FilmInformation provide..
Film Tensile Strength at Yield, MD 25.0 MPa
3630 psi
ISO 527-3
EMS-Grivory Grivory® BM 17 PA*
Product description: Grilon BM 17 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 17 natural has the following features: High flexibility and toughnessVery good ori..
Film Tensile Strength at Yield, MD 25.0 MPa
3630 psi
ASTM D882
Eastman D4032-F Polyethylene  (discontinued **)
D4032-F is a low density, fractional-melt formulation which contains no slip and medium antiblock. It is designed for film applications requiring exceptional toughness, such as in heavy-duty shippi..