Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents of 5 - 20% give a useful range of properties broadly similar to those of the polyolefins (the polyethylenes and polypropylene). They melt at lower temperatures than the homopolymer, giving a useful improvement in melt-processability. Their other properties are similar to those of PHB.They are being used for biodegradable containers (of which shampoo bottles are the most high-profile example) and other articles difficult to recycle e.g. disposable razors or medically contaminated articles.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 25.0 - 30.0 MPa
3630 - 4350 psi
Film Tensile Strength at Yield, TD 25.0 - 30.0 MPa
3630 - 4350 psi
Tensile Strength, Yield 28.0 MPa
4060 psi
Film Elongation at Break, MD 7.0 - 15 %
7.0 - 15 %
Film Elongation at Break, TD 5.0 - 10 %
5.0 - 10 %
Elongation at Break 15 %
15 %
Tensile Modulus 0.900 GPa
131 ksi
Secant Modulus, MD 0.600 - 1.00 GPa
87.0 - 145 ksi
Film
Secant Modulus, TD 0.800 - 1.20 GPa
116 - 174 ksi
Film
Izod Impact, Unnotched 1.00 J/cm
1.87 ft-lb/in
Notch Status Unknown
Thermal Properties Metric English Comments
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Thermal Conductivity 0.150 W/m-K
1.04 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
Descriptive Properties Value Comments
Chemical Resistance - Alcohols Fair
Chemical Resistance - Alkalis Poor
Chemical Resistance - Dilute Acids Fair
Chemical Resistance - Greases and Oils Good
Permeability to Oxygen @25°C 0.1-0.2 x 10-13 cm3.cm cm-2 s-1 Pa -1
Film
Permeability to Water @25°C 1000-2000 x 10-13 cm3.cm cm-2 s-1 Pa -1
Film
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved