Polymer Property : Film Tensile Strength at Yield, MD = 4000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 27.6 MPa
4000 psi
ASTM D882
LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade
Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements. Regulatory Statu..
Film Tensile Strength at Yield, MD 27.6 MPa
4000 psi
ASTM D882, A 20 in/min
Total HDPE HL 535 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release ..