Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 31.0 - 39.3 MPa
4500 - 5700 psi
ASTM D882
Honeywell Halar® High Performance E-CTFE Film  (discontinued **)
Description: Halar® is a high performance Ethylene-Chlorotrifluoroethylene (E-CTFE) film with excellent mechanical, electrical and release properties. It is non-flammable, and has outstanding chem..