Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 86.2 MPa
12500 psi
ASTM D882A
DuPont Teijin Films Melinex® 331 Polyester Film, 200 Gauge
Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod..
Film Tensile Strength at Yield, MD 86.2 MPa
12500 psi
ASTM D882A
DuPont Teijin Films Melinex® 331 Polyester Film, 300 Gauge
Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod..
Film Tensile Strength at Yield, MD 86.2 MPa
12500 psi
ASTM D882A
DuPont Teijin Films Melinex® 331 Polyester Film, 700 Gauge
Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod..
Film Tensile Strength at Yield, MD 86.2 MPa
12500 psi
ASTM D882A
DuPont Teijin Films Melinex® 331W Polyester Film, 200 Gauge
An opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings. 331W has same properties as 331 with the only ex..
Film Tensile Strength at Yield, MD 86.2 MPa
12500 psi
ASTM D882A
DuPont Teijin Films Melinex® 513P Polyester Film, 650 Gauge
Melinex® 513P is a high clarity, knurled film with excellent handling properties that is pretreated on both sides to promote adhesion to most industrial coatings.General Product Info: Melinex® 513..