Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 513P Polyester Film, 650 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 513P Polyester Film, 650 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 513P is a high clarity, knurled film with excellent handling properties that is pretreated on both sides to promote adhesion to most industrial coatings.General Product Info: Melinex® 513P is used for direct write film in electronic circuit board manufacture.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 86.2 MPa
12500 psi
ASTM D882A
Film Tensile Strength at Yield, TD 82.7 MPa
12000 psi
ASTM D882A
Coefficient of Friction, Dynamic 0.50
0.50
[in<sup>2</sup>/lb], A-B; ASTM D1894
Film Tensile Strength at Break, MD 172 MPa
25000 psi
ASTM D882A
Film Tensile Strength at Break, TD 186 MPa
27000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.40 %

@Temperature 190 °C,
Time 300 sec
0.40 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Descriptive Properties Value Comments
Absorbance 0.0007
MTM 2.34 @ 366 nM
Color -0.06
a, DuPont Test Method
1.75
b, DuPont Test Method
96.2
L, DuPont Test Method
Users viewing this material also viewed the following: