Film Tensile Strength at Yield, MD 9.31 MPa
1350 psi
at 2% offset; ASTM D882
ExxonMobil Exceed™ 1518CA Tough Premium Film Resin  (discontinued **)
Exceed 1518CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518CA resin have outstanding tensile, impact strength and puncture. These superi..
Film Tensile Strength at Yield, MD 9.31 MPa
1350 psi
at 2% offset; ASTM D882
ExxonMobil LL 3301.34 Premium High Strength Film Resin  (discontinued **)
LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi..
Film Tensile Strength at Yield, MD 9.31 MPa
1350 psi
at 2% offset; ASTM D882
ExxonMobil LL 3301.63 Premium High Strength Film Resin  (discontinued **)
LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi..