Polymer Property : Film Tensile Strength at Yield, MD = 9.40 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.10 - 9.40 MPa
1170 - 1360 psi
Average value: 8.68 MPa Grade Count:4
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..