Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.128 GPa | 18.6 ksi | 5%; ASTM-D638 |
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle.. |