Mechanical Properties Metric English Comments
Secant Modulus 0.128 GPa
18.6 ksi
5%; ASTM-D638
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding
The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle..