Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.295 GPa | 42.8 ksi | 1%; ASTM D790 |
NOVA Chemicals Novapol® LM-2522-A LDPE Injection Molding Resin Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat.. |
|||
Secant Modulus | 0.295 GPa | 42.8 ksi | 1%; ASTM D790 |
NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat.. |