Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformation provided by Nova Chemicals
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D792
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength at Break 8.20 MPa
1190 psi
ASTM D638
Tensile Strength, Yield 9.40 MPa
1360 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Secant Modulus 0.227 GPa
32.9 ksi
2%; ASTM D790
0.295 GPa
42.8 ksi
1%; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Brittleness Temperature <= -35.0 °C
<= -31.0 °F
0% Failure Rate; ASTM D746