Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 10 g
10 g
ASTM D1922
SABIC F04660 High Density Polyethylene for Blown Film Applications
Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp..
Elmendorf Tear Strength MD 10 g
10 g
ASTM D1922
LyondellBasell Alathon® L5906 High Density Polyethylene
ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high t..
Elmendorf Tear Strength MD 10 g
10 g
ASTM D1922
Formosa Plastics Formolene® E925 Film HDPE
High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E925 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics..
Elmendorf Tear Strength MD 10 g
10 g
ASTM D1922
ExxonMobil HDPE HTA 108 High Density Polyethylene Resin
Product Description: HTA 108 is a homopolymer HDPE film grade designed to improve stiffness and barrier in coextrusion or in PE blends. When blended with LLDPE, HTA 108 improves their processability..
Elmendorf Tear Strength MD 10 g
10 g
Bapolene® 1057 Polyethylene, Extrusion Coating
Bapolene 1057 is low high density polyethylene for high speed extrusion coating applications that require superior adhesion and low neck-in. It complies with US FDA 21CFR177.1520.Applications: Pouc..