Polymer Property : Elmendorf Tear Strength MD = 8.2 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 8.2 g
8.2 g
Orientation not specified; ASTM D1922-89
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme..