Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 73.8 MPa | 10700 psi | ASTM D882 |
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin
(discontinued **) Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Break, MD | 73.5 MPa | 10700 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL2764 Linear low density polyethylene resin
(discontinued **) Titanceed® mL2764 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL2764 have outstanding tensile properties, impact streng.. |
|||
Film Tensile Strength at Break, MD | 73.5 MPa | 10700 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL3564 Linear low density polyethylene resin
(discontinued **) Titanceed® mL3564 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL3564 have outstanding tensile properties, impact streng.. |
|||
Film Tensile Strength at Break, MD | 73.7 MPa | 10700 psi | |
3M 8507 Repulpable Forms-Splicing Tape 3M™ Repulpable Forms-Splicing Tape 8507 is a specially engineered tape for forms-splicing with a thin, semi-bleached backing, a heat resistant adhesive and skip-slit for easy separation; all comple.. |
|||
Film Tensile Strength at Break, MD | 73.8 MPa | 10700 psi | ASTM D882 |
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Break, MD | 73.8 MPa | 10700 psi | ASTM D882 |
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |