Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ISO 527
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
Film Tensile Strength at Break, MD 90.0 MPa

@Thickness 0.100 mm
13100 psi

@Thickness 0.00394 in
ISO 527
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 ..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E..
Film Tensile Strength at Break, MD 90.3 MPa
13100 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte™ 28MWHB OPP Film
Product Description: A multi-layer, cavitaed, white OPP film that has exceptional barrier to gases, flavors and moistures. It is metalized on one side with a proprietary sealant layer on the other. ..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ISO 527-3
EMS-Grivory Grivory® CA 6 E PA*
Product description: Grilon CA 6 E is a non-extracted copolyamide with a low melting point. Grilon CA 6 E characterizes itself through the following properties Very high flexibility and toughnessVer..
Film Tensile Strength at Break, MD 90.3 MPa
13100 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 150LL-302 OPP Film
Product Description: A white, corona-treated polypropylene label facestock designed for rigid and semi-rigid pressure-sensitive applications requiring durability, opacity, and excellent graphic appe..
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 125 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..