Film Tensile Strength at Break, MD 15.2 MPa
2200 psi
ASTM D882
LyondellBasell Petrothene® NA334000 Low Density Polyethylene
ApplicationsPETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability. Regulat..