Polymer Property : Film Tensile Strength at Break, MD = 25.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 25.4 MPa
3680 psi
ASTM D882
ExxonMobil LD 136.MV Packaging Film Resin  (discontinued **)
LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa..
Film Tensile Strength at Break, MD 25.4 MPa
3680 psi
ASTM D882
ExxonMobil LD 136.NI Packaging Film Resin  (discontinued **)
LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa..