Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
SABIC HP4023W Low Density Polyethylene for Blown Film Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE5020 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High draw down, low neck-in, excellent heat sealability, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms t.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM-D882 |
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Film Tensile Strength at Break, MD | 18.0 MPa | 2610 psi | ASTM D882 |
Huntsman PE8010 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |