Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 23.4 MPa | 3390 psi | |
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib.. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3390 psi | |
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip .. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3390 psi | |
Dow LDPE 170A Low Density Polyethylene, Blown Film Grade DOW LDPE 170A resin is used for shrink and heavy duty blown film applications where optical clarity is desired. It contains medium level of antiblock additives. It complies with U.S. FDA regulation .. |
|||
Film Tensile Strength at Break, MD | 23.4 MPa | 3390 psi | |
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re.. |