Polymer Property : Film Tensile Strength at Break, MD = 3880 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 26.8 MPa
3880 psi
ASTM D882
ExxonMobil Pax-Plus™ 3201 Blown Film Resin
Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista..