Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 15.0 - 40.0 MPa
2180 - 5800 psi
Average value: 27.1 MPa Grade Count:145
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Film Tensile Strength at Break, MD 30.0 - 40.0 MPa
4350 - 5800 psi
ISO 527-3
Borealis Borclear™ RB709CF Polypropylene Ethylene Copolymer
Borclear™ RB709CF is a propylene -ethylene copolymer. This grade is suitable for the manufacturing of unoriented film on blown film lines. Applications: Borclear™ RB709CF is recommended for seal..