Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 40.2 MPa | 5830 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin
(discontinued **) LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughne.. |
|||
Film Tensile Strength at Break, MD | 40.2 MPa | 5830 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin
(discontinued **) LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud.. |
|||
Film Tensile Strength at Break, MD | 40.2 MPa | 5830 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin
(discontinued **) LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down.. |
|||
Film Tensile Strength at Break, MD | 40.2 MPa | 5830 psi | Ultimate; ASTM D882 |
LG Chemical SEETEC ST408 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Film Tensile Strength at Break, MD | 40.2 MPa | 5830 psi | Calculated from mfr's report of 51 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® N196 Paper, 5 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |