Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical SEETEC ST408 Linear Low Density Polyethylene, Blown Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer LG Chemical
Trade Name SEETEC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC ST408 Linear Low Density Polyethylene, Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplications: Stretch wrap, food wrapCAS No. 26221-73-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.914 - 0.916 g/cc
0.914 - 0.916 g/cc
ASTM D1505
Melt Flow 2.2 - 2.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 - 2.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 750 %
750 %
ASTM D882
Elmendorf Tear Strength MD 24 g
24 g
ASTM D1922
Elmendorf Tear Strength TD 30 g
30 g
ASTM D1922
Dart Drop Test 340 g
0.750 lb
ASTM D1709
Film Tensile Strength at Break, MD 40.2 MPa
5830 psi
Ultimate; ASTM D882
Film Tensile Strength at Break, TD 34.3 MPa
4970 psi
Ultimate; ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 0.70 %
0.70 %
ASTM D1003
Gloss 155 %
155 %
45°; ASTM D2457