Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 41.4 MPa | 6000 psi | ASTM D882 |
M. Holland Company MAGMA® LL1091 LLDPE
(discontinued **) Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Film Tensile Strength at Break, MD | 41.4 - 62.1 MPa | 6000 - 9000 psi | ASTM D882 |
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 41.4 - 62.1 MPa | 6000 - 9000 psi | ASTM D882 |
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 41.4 - 55.2 MPa | 6000 - 8000 psi | ASTM D882 |
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Film Tensile Strength at Break, MD | 41.4 - 62.1 MPa | 6000 - 9000 psi | ASTM D882 |
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |
|||
Film Tensile Strength at Break, MD | 41.4 MPa | 6000 psi | ASTM D882 |
Westlake Hifor Clear SC74558 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74558 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives... |
|||
Film Tensile Strength at Break, MD | 41.4 MPa | 6000 psi | ASTM D882 |
Westlake Hifor SC74557 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produc.. |