Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil LD 103.59 Industrial Film Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade) Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal .. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa | 4200 psi | ASTM D882 |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |
|||
Film Tensile Strength at Break, MD | 29.0 MPa @Thickness 0.0381 mm |
4200 psi @Thickness 0.00150 in |
ASTM D-882 |
Bapolene® 107A Low Density Polyethylene Film Extrusion Resin Bapolene® 107A is an LDPE for blown film. It contains 3400 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p.. |