Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 43.4 MPa | 6300 psi | ASTM D882 |
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
(discontinued **) Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Break, MD | 43.4 MPa | 6300 psi | ASTM D882 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP510300 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. LP510300 is recommended .. |
|||
Film Tensile Strength at Break, MD | 43.4 MPa | 6300 psi | ASTM D882, A 20 in/min |
Total HDPE HL 535 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release .. |
|||
Film Tensile Strength at Break, MD | 43.4 MPa | 6290 psi | |
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g.. |