Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 26.2 - 31.7 MPa | 3800 - 4600 psi | ASTM D882 |
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film
(discontinued **) Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 26.2 - 31.7 MPa | 3800 - 4600 psi | ASTM D882 |
Honeywell ACLAR® Cx™ 8A Heat Sealable, Co-Extruded CTFE Film
(discontinued **) Description: ACLAR® Cx™ 8A is a heat sealable coextruded CTFE film.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 20.7 - 31.7 MPa | 3000 - 4600 psi | ASTM D882 |
Honeywell ACLAR® 33C (7.80 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |