Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 26.2 - 141 MPa
3800 - 20500 psi
Average value: 62.3 MPa Grade Count:15
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Film Tensile Strength at Break, MD 26.2 - 31.7 MPa
3800 - 4600 psi
ASTM D882
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film  (discontinued **)
Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell.
Film Tensile Strength at Break, MD 26.2 - 31.7 MPa
3800 - 4600 psi
ASTM D882
Honeywell ACLAR® Cx™ 8A Heat Sealable, Co-Extruded CTFE Film  (discontinued **)
Description: ACLAR® Cx™ 8A is a heat sealable coextruded CTFE film.Information provided by Honeywell.
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
LyondellBasell Petrothene® NA362176 Low Density Polyethylene
ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
LyondellBasell Petrothene® NA362005 Low Density Polyethylene
ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM-D882
Westlake EB171 MDPE Medium Density Polyethylene
Westlake EF171 is a MDPE resin suggested for use in shrink packaging applications. This material has good TD shrinkage, good optical properties, excellent machinability, and toughness. This resin gr..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
Westlake EF418 Low Density Polyethylene
WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
Westlake EF796 Low Density Polyethylene
Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
Westlake EF923 Low Density Polyethylene
Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
Westlake EN923 Low Density Polyethylene
Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
Westlake EP413 Low Density Polyethylene
WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LD 317.09 Film Resin
LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LD 317.87 Film Resin
LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin
Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin
Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie..
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin