Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
ASTM D882
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film)
ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b..
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
ASTM D882
Westlake EF1807 Low Density Polyethylene
Westlake Polyethylene EF1807 is a low density formulation suggested for film applications that require toughness.Application/UsesShrink filmFrozen food packagingFDA: This material complies with FDA ..
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
ASTM D882
Westlake EN1807AA Low Density Polyethylene
WESTLAKE polyethylene EN1807 is a fractional-melt low- density formulation suggested for film applications requiring high impact strength, high tear strength, and very good optical properties, such ..
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
ASTM D882
Westlake LF1021 Butene Linear Low Density Polyethylene
Westlake LF1021 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant ..
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design..
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
ASTM D882
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00119 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic..
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
510
ExxonMobil Hicor® 30 HF 104 OHD Film
One-side sealable, one-side treated, coextruded, oriented high density polyethylene film. It is ideal for use in HFFS and VFFS machines. It is designed to be used unsupported or in laminated applic..
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
ASTM D882
ExxonMobil Escorene™ FL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00119 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Ap..