Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ FL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ FL 00119 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: FL 00119 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Agricultural FilmCo-Extrusion FilmsHigh Frequency SealingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil method
Vinyl Acetate Content 19 %
19 %
ExxonMobil method
Melt Flow 0.65 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 650 %
650 %
ASTM D882
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
ASTM D882
Film Tensile Strength at Break, TD 30.3 MPa
4400 psi
ASTM D882
1% Secant Modulus, MD 53.8 MPa
7800 psi
ASTM D882
1% Secant Modulus, TD 55.8 MPa
8100 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 183 °C
<= 361 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 62.2 °C
144 °F
ASTM D1525
Users viewing this material also viewed the following: