Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ISO 527-3
Polimeri Europa Greenflex® FF 55 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 55 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 55 show high flexibility.Main Applications: Greenflex FF 55 is recommended f..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
Reliance Industries LLDPE film - Organic acid based film
Information provided by Reliance Industries
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ISO 527-3
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE  (discontinued **)
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ASTM D 882
NOVA Chemicals Novapol® PF-0318-E Butene LLDPE Film Resin
PF-0318-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ISO 527
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene
LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of ca..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ISO 1184
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film
Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ISO 1184
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film
Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ISO 527-3
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ISO 527-3
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film
Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2070D Polyethylene resin is a fully formulated linear low density polyethylene resin offering high strength and low gel properties for blown film food packaging applications. DOWLEX 2070D r..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ASTM D882
Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ASTM D882
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A..
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ASTM D882
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE  (discontinued **)