Polymer Property : Film Tensile Strength at Break, MD = 53.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Exceed™ 1327CA Blown Film Resin  (discontinued **)
Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi..
Film Tensile Strength at Break, MD 53.1 MPa

@Thickness 0.0254 mm
7700 psi

@Thickness 0.00100 in
ASTM D882A
Total 9458 HDPE Film Grade
Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba..
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LL 1001x26 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LL 1001x72 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LL 1001x74 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LL 1001x76 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil LL 1001x59 Blown Film Resin  (discontinued **)
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical