Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 38.34 MPa
5561 psi
ASTM D882
Dow DOWLEX™ 2038 Linear Low Density Polyethylene
Linear Low Density PolyethyleneInformation provided by Dow
Film Tensile Strength at Break, MD 38.34 MPa
5561 psi
ASTM D882
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene
Fast processing on narrow die gaps For blown film paper product over wrap applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow