Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 59.1 MPa
8570 psi
ASTM D5803
3M 6141 Light Duty Water Activated Paper Tape
3M™ Light Duty Water Activated Paper Tape 6141 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high-tack, water-activated, modified cornstar..