Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 59.1 MPa | 8570 psi | ASTM D5803 |
3M 6141 Light Duty Water Activated Paper Tape 3M™ Light Duty Water Activated Paper Tape 6141 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high-tack, water-activated, modified cornstar.. |