Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 42.13 MPa | 6111 psi | 510 |
ExxonMobil Label-Lyte® 90 LP Coated, High Sheen, Metallized, White Opaque OPP for Water-based Patch Label Applications Coated, white, metallized polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. This film is compatible with offset litho and UV-cured in.. |
|||
Film Tensile Strength at Break, MD | 42.13 MPa | 6111 psi | 510 |
ExxonMobil Label-Lyte® 95 LP Coated, White Opaque OPP for Water-based Patch Label Applications White, polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement on glass, metal, HDPE, and PET containers. It is designed to be used as a mon.. |