Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 66.2 MPa
9600 psi
ASTM D882
Westlake Mxsten CV77529 Polyethylene Plastomer
Mxsten CV plastomer CV77529 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this ..
Film Tensile Strength at Break, MD 66.2 MPa
9600 psi
ASTM D882
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Break, MD 66.2 MPa
9600 psi
ASTM D882
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin
Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit..
Film Tensile Strength at Break, MD 66.2 MPa
9600 psi
ASTM D882
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin
Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st..
Film Tensile Strength at Break, MD 66.2 MPa
9600 psi
ASTM D882
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..