Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 46.2 MPa | 6700 psi | |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |