Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 69.0 MPa | 10000 psi | ASTM D882 |
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar®EZS is a high slip version of EZ. Used where a premium product appearance i.. |
|||
Film Tensile Strength at Break, MD | 69.0 MPa | 10000 psi | ASTM D882 |
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar®EZS is a high slip version of EZ. Used where a premium product appearance i.. |
|||
Film Tensile Strength at Break, MD | 69.0 MPa | 10000 psi | ASTM D882 |
DuPont™ Clysar® VEZ Polyolefin Shrink Packaging Film, 50 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.DuPont Clysar® VEZ is a clear, biaxially oriented, heat-shrinkable, multilayer film with one of the lowest shrink force available in the Clysar® line. C.. |
|||
Film Tensile Strength at Break, MD | 69.0 MPa | 10000 psi | ASTM D882 |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Film Tensile Strength at Break, MD | 69.0 MPa | 10000 psi | ASTM D882 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Film Tensile Strength at Break, MD | 69.0 MPa | 10000 psi | ASTM D882 |
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 50 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar® EZS is a high slip version of EZ. Used where a premium product appearance .. |