Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 7.76 MPa | 1130 psi | ASTM D3759 |
3M Scotch® 375 Superior Performance Box Sealing Tape Scotch® Box Sealing Tape 375 is a superior performance packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. The product has the strongest conformab.. |
|||
Film Tensile Strength at Break, MD | 7.76 MPa | 1130 psi | ASTM D3759 |
3M Scotch® 3785 Performance Continuous Taping System Tape Scotch® Performance Continuous Taping System Tapes 3785 is a packaging tape used for box sealing and specially designed for use with the 3M-Matic™ Continuous Taping System (CTS) stand. These tapes.. |