Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 40.0 - 60.0 MPa | 5800 - 8700 psi | ISO 527-3 |
Borealis BA11CF Polypropylene Copolymer BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. .. |
|||
Film Tensile Strength at Break, MD | 40.0 - 60.0 MPa | 5800 - 8700 psi | ISO 527-3 |
Borealis BB213CF Polypropylene Copolymer BB213CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BB213CF is recommended for food packaging.. |