Polymer Property : Film Tensile Strength at Break, MD = 8900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD >= 61.4 MPa
>= 8900 psi
ASTM D 882 A
Total 1285 HDPE film
Applications: T-shirt sacks, trash can liners, merchandise bags, coex applicationsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
Westlake Hifor Xtreme SC74836 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme Polyethylene SC74836 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock and processing aid. Films..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
ExxonMobil LL 3201.69 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin
Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The..
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
Westlake Hifor Xtreme SC74859 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74859 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and high processing aid.Application/U..