Polymer Property : Tensile Strength, Yield = 0.979 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.979 MPa

@Strain 100 %
142 psi

@Strain 100 %
ASTM D412
Multibase Multi-Flex® G 7705 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tensile Strength, Yield 0.979 MPa
142 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7272 Butyl and Halobutyl Rubber
General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc.