Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.65 MPa | 240 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-235 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.65 MPa | 240 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-235 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.65 MPa | 240 psi | ASTM D412 |
Teknor Apex UNIPRENE® 2005 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 1.65 MPa | 240 psi | at 150% Elongation, maximum |
Dow Corning SILASTIC® LSR 9682-50 PARTS A&B 50 Durometer, 2-part, 1 to 1 mix, clear Liquid Silicone RubberInformation provided by Dow Corning |