Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.97 MPa | 285 psi | 200%, post cured- 8 hours at 200°C; ASTM D412 |
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 1.97 MPa | 286 psi | ASTM D412 |
Polymax® Maxelast® P1745N TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 1.97 MPa | 286 psi | ASTM D412 |
Polymax® Maxelast® P2635 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 1.97 MPa | 285 psi | at 100% secant; ASTM D638 |
Multibase Multi-Flex® A 5703 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 1.97 MPa | 285 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7265D Fluorocarbon-Elastomer Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.97 MPa | 285 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7336 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.97 MPa @Strain 100 % |
286 psi @Strain 100 % |
|
Saint-Gobain Tygon® E-1000 Ultra-Soft Laboratory Tubing Soft and flexible, Tygon® E-1000 Non-DEHP laboratory tubing delivers the same performance in a formulation that contains non-DEHP [Bis (2-ethylhexyl) phthalate] plasticizers. The market demand a.. |